Recommendations Regarding Joint Fillers
DEFER JOINT FILLING AS LONG AS POSSIBLE TO MINIMIZE THE EFFECTS OF “DRYING SHRINKAGE RELATED JOINT…

STRUX® 90/40 Replaces WWF as Minimum Reinforcing for Composite Steel Floor Deck Construction Technical Bulletin – TB-0003
Composite metal deck is a cost-effective flooring system used in many multi-story buildings. Floors constructed of…

Cracking of Masonry Walls Technical Bulletin – TB-0007B
The DRY-BLOCK® System of admixtures for concrete masonry units (CMU) and mortar is an effective water-repellent…

CRACK REPAIR PROCEDURE – Narrower Than 0.016in
TOOLS 4″ & 6” Right Angled Grinders. 1/8″ W X 3-1/2″ Dia. smooth rim diamond blade.…

DUCTILCRETE® Engineered Slab System Post-Installation Guide
Joint Treatment and Maintenance The Floor has a five (5) year limited warranty that requires the…

How DCI® Works – TB-0909
This Technical Bulletin describes the role of corrosion inhibitors, and the way DCI® Corrosion Inhibitor controls…

CRACK STITCHING PROCEDURE
TOOLS & MATERIALS 1. Vacuum. 2. Hammer Drill and a 3. 5/16”” diameter x 6” long drill…

DUCTILCRETE® Staining & Polishing Procedure
This Procedure can be utilized to darken the surface of the DUCTILCRETE® when grinding and/or polishing edges…

CRACK REPAIR PROCEDURE – Min Width 0.016in
TOOLS 4″ Right Angle Grinder. Diamond V Blade (3/8” wide). Norton Blue Strip Disc (No substitutes).…

Understanding Cracks in Residential Concrete; Control and Prevention
Cracks in concrete come in many sizes and shapes: from superficial but aesthetically displeasing surface cracks,…

Is offsite construction the answer to jobsite safety concerns?
Prior to the pandemic, there was already a push toward offsite construction to reduce labor costs…

DUCTILCRETE® Pocket Handbook
System Information CS100 Dual layer, wet-on-wet system Topping slab must be a minimum 3”, although there…